Detailed welding characteristics of aluminum and aluminum alloys

Weld characteristics of aluminum and aluminum alloy pipe lateral tee dimension,
(1) Aluminum is liable to be oxidized in air or welding, and the formed alumina (Al2O3)  has high melting point, high stability and difficult to remove. It prevents melting and melting of the base metal. It has a large proportion of oxide film, it is not easy to float from the surface, it is easy to form defects such as slag inclusions, not molten, insufficient penetration and the like. Surface oxide film of aluminum and adsorption of a large amount of moisture easily cause pores in the weld. Before welding to remove the oxide on the surface, chemical or mechanical methods must be used for rigorous surface cleaning. It enhances protection during the welding process and prevents oxidation. In the case of tungsten argon arc welding, an AC power supply is selected to remove the oxide film by "cathode cleaning". For gas welding use flux to remove oxide film. For thick plate welding, welding heat can be increased, such as when the arc heat is large, helium gas or argon-helium mixed gas protection is used, or large-scale melt gas shield welding is used. For DC positive connections, "cathode" is not required. clean up. "
(2) The thermal conductivity and specific heat capacity of aluminum and aluminum alloy are more than twice that of carbon steel and low alloy steel. The thermal conductivity of aluminum is 10 times the thermal conductivity of austenitic stainless steel. During the welding process, a large amount of heat is rapidly transferred to the interior of the base metal. Thus, when welding aluminum and aluminum alloys, energy is consumed in addition to the molten metal pool, and more heat is consumed in other parts of the metal. Useless energy consumption is more important than steel. In order to obtain a welded joint of high quality, it is necessary to use the energy concentration and high energy source as much as possible, and in some cases technical means such as preheating can be used.

(3) The linear expansion coefficient of aluminum and aluminum alloy is about twice the linear expansion coefficient of carbon steel and low alloy steel. As aluminum solidifies, the volumetric shrinkage rate increases and the deformation and stress of the weld becomes large. Therefore, measures to prevent welding deformation are required. Shrinkage, contraction, high temperature cracking and high internal stress are likely to occur when the aluminum weld pool solidifies. In production it is possible to use means for adjusting the composition of the wire and the welding process to prevent the occurrence of hot cracks. Where corrosion resistance is observed, an aluminum alloy other than the aluminum-magnesium alloy may be welded using an aluminum-silicon alloy wire. If the aluminum containing silicon alloy contains 0.5% silicon, the tendency to pyrolysis is greater. As the silicon content increases, the crystallization temperature range of the alloy becomes smaller, the flowability is remarkably improved, the shrinkage rate decreases, and the tendency to pyrolysis decreases accordingly. According to manufacturing experience, the use of SAISi strips (silicon content 4.5 to 6%) has better crack resistance since pyrolysis does not occur when containing 5 to 6% of silicon.
(4) Aluminum has strong reflectivity against light and heat. There is no obvious color change when solids and liquid are migrating and it is difficult to judge during the welding operation. High temperature aluminum has low strength, it is difficult to support the molten pool, and welding is easy.
(5) Aluminum and aluminum alloys can dissolve a large amount of hydrogen in a liquid state, and solid state hardly dissolves hydrogen. In the process of solidification and quenching of the weld pool, hydrogen does not have time to overflow and hydrogen holes tend to form. Moisture in the arc columnar atmosphere, welding material adsorbed on the oxide film on the surface of the base material and moisture are all important sources of hydrogen in the weld. Therefore, the hydrogen source must be tightly controlled to prevent the formation of pores.
(6) The alloying element evaporates and easily burns, and the welding performance deteriorates.
(7) If deformation reinforcement or solid solution strengthening is applied to the base material of the base metal, the strength of the heat affected zone may decrease due to the welding heat.
(8) Aluminum is a face centered cubic lattice without isomers. There is no phase change between heating and cooling. Weld grains tend to become coarse and not refined by phase transformation.